What defects will appear in the billet during continuous casting
Continuous casting is only a problem of keeping and impossible to correct steelmaking and equipment. In the whole operation, there will be some defects in the billet, which affects the normal production. This is what we need to pay attention to, understand the specific types, in order to better operate.

Billet defects:
- Corner crack. After serious wear of the lower mouth of the mould fittings, a large air gap is formed between the copper tube of the mould and the billet, which results in too weak cooling and thinning of the shell. The cooling gradient is too large and the stress is concentrated.
- Intermediate cracks. When the billet passes through the secondary cooling zone, the cooling is not uniform, and the thermal stress produced by the excessive temperature rise exceeds the maximum stress between the columnar crystals, and the development of the columnar crystals increases the probability of forming the intermediate cracks.
- Crackunder pressure. The pressure of the roller is too high, which makes the solid-liquid two-phase zone of the solidified billet produce the crack under pressure. For the cast billet with cylindrical crystal developed and intermediate crack, a large crack under pressure is often formed along the direction of the billet.
- The center is loose. The columnar crystal on both sides of the billet grows to the center, which results in “bypass “, which prevents the molten steel above the bridge from solidification and shrinkage of the molten steel under the bridge. When the molten steel under the bridge solidifies, many small pores are left.

It is especially pointed out that the longitudinal crack on the billet surface originates from the lens fittings, is uneven in the thickness of the primary shell in the meniscus area, and the tensile stress acting on the shell exceeds the high temperature allowable strength and strain of the steel.
Contact Us
Address
High-tech Industrial Development Zone, Zhengzhou City, Henan Province, China.
jean@ji-steel.com
Phone
+86 188 3804 2177
Products
- Continuous Casting
- ● Copper Mould Tube
- ● Mould Assembly
- Steel Melting
- ● Graphite Electrode
- Refractory Material
- ● Nozzle Bricks
- ● Magnesia Carbon Brick
- ● High Alumina Brick
Contact
- jean@ji-steel.com
- +86 371 6781 0168
- +86 188 3804 2177
- +86 188 3804 2177
- www.ji-steel.com
- High-tech Industrial Development Zone, Zhengzhou City, Henan Province, China.
Quick Links
© Copyright 2022 JI Steel. All right reserved.